MOLYKOTE 7365

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE 7365

Main features

  • Friction-Stabilizing Brake Formulations
  • 3 to 7 Weight-Percent Blending
  • Up to 650 deg C Application

Product Description

MOLYKOTE 7365 Lubolid (EXP) Additive Powder is a free-flowing gray blend of inorganic solids for friction-lining formulations. This grade is used for friction stabilization, primarily in passenger-car disc brake pads. The powder may be added at a recommended 3 to 7 weight percent and mixed to homogeneous distribution within supported formulations. Its application-temperature limit is 650 deg C. The powder has a tamped density of 0.43 g/cm3, 0.9% residue on a 100 micron screen and 1.0% maximum moisture. These are additive-powder properties, not finished brake-system performance ratings.

Key features

  • Friction-stabilizing additive role: Provides an inorganic-solids additive option for friction stabilization in supported brake formulations.
  • 3 to 7 weight-percent blending: Add within this recommended range, then mix to homogeneous distribution.
  • Up to 650 deg C application: Has this maximum application temperature for supported friction-lining formulations.

Applications

Passenger-car disc brake pads are the main application, with supported use also covering disc, drum, rail and industrial brake or clutch lining formulations.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Gray
Density (g)
3.26 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values are exact to MOLYKOTE 7365 Lubolid (EXP) Additive Powder.

PropertyValueUnitMethod / condition
ColorGray-Typical; as supplied
ConsistencyFree-flowing powder-Typical; as supplied
Tamped volume233ml/100 gTypical; exact 7365 grade
Tamped density0.43g/cm3Typical; exact 7365 grade
Theoretical density3.26g/cm3Typical; exact 7365 grade
Residue on 100 micron screen0.9%Typical; exact 7365 grade
Moisture1.0 maximum%Typical; exact 7365 grade
Usable life60monthsOriginal unopened bag at or below 25 deg C