LOCTITE SI 5049

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE SI 5049

Main features

  • 8 to 10 Minute Tack-Free Time
  • At Least 400% Cured Elongation
  • -34 to 204 deg C Temperature Exposure

Product Description

LOCTITE SI 5049 is a one-part, thixotropic acetoxy silicone paste that cures by room-temperature vulcanization for potting, sealing, and coating applications. The sealant reaches a tack-free surface in 8 to 10 minutes at 25 deg C and 50 +/- 5% relative humidity. After 7 days under the same conditions, cured material has at least 400% elongation at break, at least 0.8 N/mm^2 tensile strength, and Shore A hardness of at least 11. It permits water contact 2 hours after application and has a stated temperature range of -34 to 204 deg C.

Key features

  • 8 to 10 Minute Tack-Free Time: Tack-free surface at 25 deg C and 50 +/- 5% relative humidity.
  • At Least 400% Cured Elongation: Elongation at break after 7 days at 25 deg C and 50% relative humidity.
  • Post-Application Water Contact: Water contact is supported 2 hours after application.

Applications

Potting, sealing, coating, and supported bonding to glass, ceramics, aluminum, primed steel, and some plastics.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear paste and lump free
Chemistry Type
Acetoxy silicone
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.02 - 1.07
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
400 %

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
Specific gravity1.02 to 1.07LMS; 25 deg C
Extrusion rateAt least 130g/minLMS; Semco cartridge, 0.63 MPa, 2 h, 25 deg C
FlowUp to 12.7mmLMS; ISO 7390, after 2 min
Technical properties

Cured material

PropertyValueUnitMethod / condition
Shore hardnessAt least 11Shore ALMS; ISO 868, 7 days at 25 deg C / 50% RH
Elongation at breakAt least 400%LMS; ISO 37, 7 days at 25 deg C / 50% RH
Tensile strengthAt least 0.8N/mm^2LMS; ISO 37, 7 days at 25 deg C / 50% RH